Benang Fiberglass Disesuaikan Kanthi TEX saka 33 nganti 200TEX
Diameter Benang (um) | Kode layang | Speksifikasi tipikal |
9 | G | G37, G67, G75, G150 |
7 | E | E110, E225 |
6 | DE | DE75, DE300 |
5 | D | D450, D900 |
DATA TEKNIS
Benang jinis pati
Bulu kurang sajrone unwinding, kinerja tenun sing apik banget, gampang disizing, suhu dekomposisi kurang, residu awu sing sithik, permukaan putih lan rata saka kain sing diasilake
sebutan IPC | Diameter benang | Kapadhetan linear | isi Kelembapan | Bisa kobong |
G37 | ± 10 | 137.0±3.0 | ≤0.10 | 1.10±0.15 |
G67 | ± 10 | 74.6±2.5 | ≤0.10 | 1.10±0.15 |
G75 | ± 10 | 68.9±2.5 | ≤0.10 | 1.10±0.15 |
G150 | ± 10 | 33.7±4.0 | ≤0.10 | 1.05±0.15 |
E110 | ± 10 | 44.9±3.0 | ≤0.10 | 1.20±0.15 |
E225 | ± 10 | 22.5±4.0 | ≤0.10 | 1.15±0.20 |
DE75 | ± 10 | 68.9±2.5 | ≤0.10 | 1.15±0.20 |
DE300 | ± 10 | 16.9±5.0 | ≤0.10 | 1.30±0.30 |
D450 | ± 10 | 11.2±5.5 | ≤0.10 | 1.30±0.25 |
D900 | ± 10 | 5.6±5.5 | ≤0.10 | 1.45±0.30 |